Aluminum Doped Zinc Oxide Layers by Atomic Layer Deposition and Magnetron Sputtering: Formation and Comparison of Optoelectronic Properties

in: Physical Sciences and Technology (2016)
Mussabek, Gauhar K.; Dikhanbayev, Kadyrjan K.; Sivakov, Vladimir; Talkenberg, Florian; Sailaubek, S.; Djunusbekov, A.S.; Ukenova, G.Ye.; Kemelbekova, A.Ye.
Thin films of aluminum-doped zinc oxide (AZO) were prepared using magnetron sputtering and atomic layer deposition (ALD) techniques. Atomic force microscopy (AFM) studies of AZO films surface morphology show that the surface of produced by ALD films is a smoother in comparison with films formed by magnetron sputtering. According to comparative analysis of optical transmittance spectra in the visible range of 300 - 800 nm, films formed by ALD technique demonstrates 10% higher transparency than those that obtained by magnetron sputtering. Investigation of samples electrical properties show that the conductivity of AZO films obtained by ALD technique actually two orders of magnitude higher than analogues obtained by magnetron sputtering.

Cookies & Skripte von Drittanbietern

Diese Website verwendet Cookies. Für eine optimale Performance, eine reibungslose Verwendung sozialer Medien und aus Werbezwecken empfiehlt es sich, der Verwendung von Cookies & Skripten durch Drittanbieter zuzustimmen. Dafür werden möglicherweise Informationen zu Ihrer Verwendung der Website von Drittanbietern für soziale Medien, Werbung und Analysen weitergegeben.
Weitere Informationen finden Sie unter Datenschutz und im Impressum.
Welchen Cookies & Skripten und der damit verbundenen Verarbeitung Ihrer persönlichen Daten stimmen Sie zu?

Sie können Ihre Einstellungen jederzeit unter Datenschutz ändern.