Spatial homogeneity of superconducting order parameter in NbN films grown by atomic layer deposition

in: Superconductor Science & Technology (2026)
Linzen, Sven Peter; Ziegler, Mario; Oelsner, Gregor; Stolz, Ronny; Ilichev, Evgeni; Lorenz, J.; Tautz, F. S.; Lüpke, F.
Due to their high kinetic inductance, highly disordered superconducting thin films are a potential hardware for the realization of compact, low-noise elements in cryoelectronic applications. However, high disorder typically results in structural defects that cause spatial inhomogeneity of the superconducting order parameter, thereby impairing the film’s properties. Here, we employ scanning tunneling microscopy to demonstrate that NbN thin films fabricated by plasma-enhanced atomic layer deposition (PE-ALD) exhibit unusual spatial homogeneity, even at thicknesses approaching the superconductor-insulator transition. Tunneling spectra acquired across the sample surface show only small variations of the order parameter with a standard deviation of 2 − 3%, on length scales that significantly exceed the film’s grain size. At the same time, the films achieve a relatively high sheet resistance (up to 1400 Ohm) and, consequently, a high sheet kinetic inductance (up to approximately 200 pH), making them well-suited for applications.

Cookies & Skripte von Drittanbietern

Diese Website verwendet Cookies. Für eine optimale Performance, eine reibungslose Verwendung sozialer Medien und aus Werbezwecken empfiehlt es sich, der Verwendung von Cookies & Skripten durch Drittanbieter zuzustimmen. Dafür werden möglicherweise Informationen zu Ihrer Verwendung der Website von Drittanbietern für soziale Medien, Werbung und Analysen weitergegeben.
Weitere Informationen finden Sie unter Datenschutz und im Impressum.
Welchen Cookies & Skripten und der damit verbundenen Verarbeitung Ihrer persönlichen Daten stimmen Sie zu?

Sie können Ihre Einstellungen jederzeit unter Datenschutz ändern.