Signatures of Dynes density of states in the terahertz response of atomic layer deposition grown superconducting NbN thin films

in: Physical Review B (2026)
Bolle, Frederik; Lin, Yayi; Saritas, Ozan; Dressel, Martin; Padurariu, Ciprian; Vegesna, Sahitya V.; Yerra, Nitesh; Krüger, Heidemarie; Scheffler, Franziska
The frequency-dependent complex optical conductivity σ ̂ ( f ) reflects key properties of superconductors, such as the energy gap 2 Δ in the density of states (DOS) and the superfluid density n s . For disordered superconductors, σ ̂ ( f ) often can be described within Bardeen-Cooper-Schrieffer (BCS) theory, while in corresponding tunneling experiments, deviations in the observed DOS typically require modeling by the phenomenological Dynes formula. The implications of such Dynes DOS for optics have been rarely discussed so far. Here we probe the terahertz σ ̂ ( f ) of superconducting NbN thin films with thicknesses ranging from 4.5 to 20 nm, which were grown by atomic layer deposition. Our frequency range from 0.3 to 2.1 THz covers energies below and above 2 Δ . For 20-nm-thick NbN, we find in σ ̂ ( f ) distinct deviations from the BCS model, including a steplike characteristic in the absorption at Δ 0 , i.e., half the zero-temperature spectral gap. These observations can be fully captured by introducing a small and temperature-independent Dynes pair-breaking rate Γ ∼ 0.036 Δ 0 . For the other films, we also observe signs of Dynes-type DOS and we discuss the evolution of 2 Δ 0 , n s , 0 , and Γ as a function of film thickness.

Cookies & Skripte von Drittanbietern

Diese Website verwendet Cookies. Für eine optimale Performance, eine reibungslose Verwendung sozialer Medien und aus Werbezwecken empfiehlt es sich, der Verwendung von Cookies & Skripten durch Drittanbieter zuzustimmen. Dafür werden möglicherweise Informationen zu Ihrer Verwendung der Website von Drittanbietern für soziale Medien, Werbung und Analysen weitergegeben.
Weitere Informationen finden Sie unter Datenschutz und im Impressum.
Welchen Cookies & Skripten und der damit verbundenen Verarbeitung Ihrer persönlichen Daten stimmen Sie zu?

Sie können Ihre Einstellungen jederzeit unter Datenschutz ändern.